Key takeaways

- Specify Ra only where function demands it; default to general notes for the rest.
- Ra 3.2 µm is a practical default for CNC machined surfaces; 0.8 µm adds cost.
- State the evaluation length and cutoff, or the supplier may measure differently.
- Ra is an average; a single deep scratch can pass Ra but fail function.
- Match the callout to the process: turning, milling, grinding and EDM differ.
Surface roughness Ra is a single number on a drawing, but it carries process, cost and inspection consequences. A callout of Ra 0.8 µm instead of Ra 3.2 µm can change the machine, the cycle time and the quote. Specifying it correctly means matching the number to the function, the process and the measurement method.
This guide covers how to specify surface roughness Ra on drawings for CNC machined, molded and fabricated parts. It explains what Ra actually measures, which processes reach which values, and how to write a callout that a supplier can quote and inspect without ambiguity.
It is written for design engineers and sourcing leads preparing an RFQ. The goal is a drawing that communicates intent, so quotes come back comparable and parts arrive to spec.
What Ra actually measures, and what it does not
Ra is the arithmetic average deviation of the roughness profile from the mean line over the evaluation length. It is a single amplitude number. It says nothing about the shape, spacing or direction of the peaks and valleys.
Two surfaces can share the same Ra and behave differently. A plateau surface with scattered deep valleys and a uniform scratched surface may both read Ra 1.6 µm. One seals, the other leaks. Ra is useful for comparison and process control, not as a complete functional description.
Ra also depends on the measurement setup. Cutoff length, evaluation length, filter and stylus tip all affect the result. ISO 4287 and ISO 4288 define the standard conditions. If the drawing does not state them, two inspectors can measure the same surface and report different Ra values.
How to write the Ra callout on a drawing
A complete callout does four things: it names the parameter, gives the value and unit, points to the surface, and states the measurement condition. Put the general requirement in the title block or a general note, and use local callouts only for surfaces that differ.
A practical general note reads: "Unless otherwise specified, machined surfaces Ra 3.2 µm, measured per ISO 4287, cutoff 0.8 mm." This covers most non-functional surfaces and keeps the drawing readable. Local callouts then mark sealing faces, bearing seats, sliding surfaces and optical or fluid-contact areas.
Use the ISO 1302 surface texture symbol for local callouts. Place the value before the symbol and the process or allowance after it where relevant. Avoid stacking multiple Ra values on one surface; if a surface has a functional requirement, state it once and clearly.
- State the parameter: Ra, not just a number.
- State the unit: µm, even though it is implied.
- State the cutoff and evaluation length, or reference the standard.
- State the measurement direction relative to lay where it matters.
- State the process where the surface is process-dependent, such as ground or EDM.
Which processes reach which Ra values
The table below gives typical achievable Ra ranges for common processes. Ranges are practical production values, not laboratory bests. Actual results depend on material, tooling, geometry and setup.
| Process | Typical achievable Ra (µm) | Notes |
|---|---|---|
| CNC turning | 0.8 – 3.2 | Finish depends on feed, nose radius and speed; finer feeds improve Ra. |
| CNC milling | 0.8 – 3.2 | Ball-nose finishing and high-speed paths reach the finer end. |
| Surface grinding | 0.2 – 0.8 | Used for flat sealing faces and bearing seats. |
| Cylindrical grinding | 0.1 – 0.4 | Shafts and bores with tight size and finish. |
| Honing | 0.1 – 0.4 | Bores requiring a controlled cross-hatch. |
| EDM (die-sinking) | 0.4 – 3.2 | Finish set by the final spark pass; recast layer remains. |
| Injection molding (tool) | 0.2 – 1.6 | Part surface copies the tool; texture specs use SPI/VDI grades. |
| Sheet metal (laser, bend) | 3.2 – 12.5 | Ra callouts rarely apply; edge and flatness dominate. |
Matching the callout to the process is the single biggest lever on cost. Asking for Ra 0.4 µm on a milled pocket forces a secondary grinding or lapping operation. Asking for Ra 3.2 µm on a sealing face may not seal.
Cost drivers: where Ra changes the quote
Surface finish is a cost driver because it changes the process, not just the pass. Moving from Ra 3.2 µm to Ra 1.6 µm on a milled face may only require a finishing pass with a sharper tool and lighter stepover. Moving to Ra 0.4 µm usually requires grinding, lapping or a dedicated finishing operation, plus handling and cleaning between steps.
The main cost factors are the number of surfaces with tight Ra, the geometry of those surfaces, the material, and whether the finish can be achieved in the same setup. Deep pockets, internal corners and interrupted cuts are harder to finish and inspect. Hardened or gummy materials add tool wear and cycle time.
Inspection cost also rises. A Ra 3.2 µm general note is checked by comparison or spot measurement. A Ra 0.2 µm callout on a critical face requires a calibrated profilometer, a defined measurement location and often a inspection report per batch. That measurement time appears in the piece price.
To control cost, specify the coarsest Ra that satisfies the function. Group surfaces with the same requirement into one general note. Reserve tight callouts for sealing, bearing, sliding and fluid-contact faces, and state the measurement location so inspection is repeatable.
Quality inspection and tolerances for Ra
Ra is inspected with a stylus profilometer or, for some surfaces, an optical instrument. The measurement must follow the drawing: same cutoff, same evaluation length, same direction. Without that, acceptance becomes a negotiation.
Define the measurement location on the drawing or in a inspection plan. A small hatched zone or a datum-relative note is enough. For large surfaces, state how many readings and where. For curved or inaccessible surfaces, agree on a replica or comparator method before production.
Set acceptance sensibly. Ra is an average, so a single deep scratch can pass Ra and still fail function. Where function is critical, add a requirement on Rz or Rmax alongside Ra, or specify a visual acceptance standard. For sealing faces, a surface texture requirement alone may not predict leak rate; a functional test is more reliable.
Ask the supplier for the measurement instrument, calibration status and report format at RFQ stage. A supplier that cannot state its cutoff and filter will struggle to hold a tight Ra callout consistently.
How to choose and audit a supplier for surface finish
Surface finish capability is a good proxy for a supplier's process control. A shop that can hold Ra 0.8 µm on a production basis has calibrated machines, defined tooling and a measurement routine. A shop that quotes Ra 0.4 µm without asking about geometry is guessing.
Use the RFQ to test this. State the Ra requirement and the measurement standard, and ask the supplier to confirm the process route, the expected Ra per operation and the inspection method. Compare answers across suppliers; the ones that ask about function and measurement location are usually the ones that can hold the callout.
During audit, check four things: the profilometer and its calibration records, the inspection plan that references the drawing's cutoff and evaluation length, the process route that achieves the finish, and the handling and cleaning steps that protect finished surfaces. Ask to see a recent inspection report for a part with a similar Ra callout.
JX Manufacturing machines, molds and fabricates parts in Dongguan, Guangdong, and quotes within 24 hours with no MOQ. If you have a drawing with Ra callouts, upload the CAD and state the functional surfaces; the process route and inspection plan can be confirmed before you commit.
Conclusion
Specifying Ra well is a matter of matching the number to the function and the process. State the parameter, the value, the cutoff and the measurement location. Reserve tight callouts for surfaces that need them, and confirm the supplier can measure what you specified.
If you are preparing an RFQ, upload your CAD and drawing notes. JX Manufacturing will review the Ra callouts, confirm the process route and return a quote within 24 hours.
FAQ
What is a good Ra value for CNC machined parts?
Ra 3.2 µm is a practical default for general CNC milled and turned surfaces. Ra 1.6 µm is common for functional faces and adds a finishing pass. Ra 0.8 µm and finer usually require grinding, lapping or a dedicated finishing operation, so specify it only where the function demands it.
How do I write an Ra callout on a drawing?
State the parameter, value and unit, and reference the measurement standard. A general note such as "machined surfaces Ra 3.2 µm per ISO 4287, cutoff 0.8 mm" covers most surfaces. Use local ISO 1302 symbols for sealing, bearing or sliding faces that need a different value, and state the measurement location.
Does a tighter Ra always cost more?
Usually yes, because tighter Ra changes the process rather than just the pass. Moving from Ra 3.2 to 1.6 µm may only need a finishing pass. Moving to Ra 0.4 µm typically requires grinding or lapping, extra handling and more inspection time, all of which appear in the piece price.
What is the difference between Ra and Rz?
Ra is the arithmetic average deviation over the evaluation length. Rz is the average of the maximum peak-to-valley heights within each sampling length. Ra is more stable and common for process control; Rz is more sensitive to isolated deep valleys, so it is often added for sealing or fatigue-critical surfaces.
Can a supplier hold Ra 0.4 µm on a milled surface?
It depends on geometry and material. Some shops can reach Ra 0.4 µm on flat, accessible milled faces with fine finishing passes, but internal corners and deep pockets usually need a secondary operation. Ask the supplier to state the process route and inspection method before you commit to the callout.